Appeal No. 95-2881 Application No. 07/988,037 This is a decision on an appeal from the final rejection of claims 6 through 10 and 17 which are all of the claims remaining in the application. The subject matter on appeal relates to a carbon fiber which has been coated with an aromatic polysulfone resin and then heated at 300-400EC for from 1 to 20 hours. Further details of this appealed subject matter are readily apparent from a review of illustrative independent claim 6 which reads as follows: 6. A carbon fiber which has been surface-coated with an aromatic polysulfone resin and then heated at 300-400EC for from 1 to 20 hours prior to any blending or mixing of said fiber with any other material. The references relied upon by the examiner as evidence of obviousness are: Turton et al. 3,785,916 Jan. 15, 1974 (Turton) Hannah et al. 3,798,105 Mar. 19, 1974 (Hannah) Hara et al. 4,764,427 Aug. 16, 1988 (Hara) Cogswell et al. 4,783,349 Nov. 8, 1988 (Cogswell) Tobukuro et al. 56-90837 Jul. 23, 1981 (Japanese '837) (JP) 2Page: Previous 1 2 3 4 5 6 NextLast modified: November 3, 2007