Appeal No. 96-1238 Application 08/082,177 component having an iodine value of less than 10, and ii) from about 20% to about 75% by weight of a beta prime phase tending hardstock component, crystallized in beta form, having an iodine value of less than about 10, said hardstock blend comprising from about 10% to about 20% by weight of said plastic shortening; c) from 0 to about 500 per million by weight of an antioxidant, and d) an effective amount of an emulsifieer; 2) injecting from about 12% to about 23% of an inert gas, under a pressure of from aout 50 to about 700 pounds per square inch to form a shortening mixture; 3) rapidly cooling said shortening mixture in a scaped wall heat exchanger in less that about 60 seconds to a temperatur of rom about 40EF (4.4EC) to about 70EF (21.1EC) while maintaining a pressure of from about 50 to about 700 psig; 4) agitating said shortening mixture and imparting enough work input in a picker box for from about 1 to about 8 minutes to transform said shortening mixture to at least 50% beta crystals upon filling, said shortening mixture having a -3-Page: Previous 1 2 3 4 5 6 7 8 9 10 NextLast modified: November 3, 2007