               52. A propylene polymer having such properties that:                   
               a melt flow rate (MFR) of said polymer at 230EC under a                
          load of 2.16 kg is in the range of 0.1 to 500 g/10 min,                     
               a pentad isotacticity M  obtained from the following                   
                                      5                                               
          formula (1) using absorption intensity Pmmmm and Pw in a C-13                 
          NMR spectrum of a boiled heptane-insoluble component contained              
          in said polymer is in the range of 0.970 to 0.995,                          
               a pentad tacticity M  obtained from the following formula              
                                   3                                                  
          (2) using absorption intensity Pmmrm, Pmrmr, Pmrrr, Prmrr,                  
          Prmmr, Prrrr and Pw in a C-NMR spectrum of a boiled heptane-13                                                 
          insoluble component contained in said polymer is in the range               
          of 0.0020 to 0.0050, and                                                    
               a crystallinity of a boiled heptane-insoluble component                
          contained in said polymer is 65% to about 79.3%;                            
                                     M  = Pmmmm                                       
                                      5                                               
            Pw                         (1)                                            
          wherein                                                                     
               Pmmmm is absorption intensity of methyl groups present in              
          the third unit among continuous five propylene units which are              
          bonded to each other with meso form, and                                    
               Pw is absorption intensity of all methyl groups in a                   
          propylene unit;                                                             
          M  =        Pmmrm + Pmrmr + Pmrrr + Prmrr + Prmmr + Prrrr                   
           3                                                                          
                                        Pw                            (2)             
          wherein                                                                     
               Pmmrm is absorption intensity of methyl groups present in              
          the third unit among continuous five propylene units                        
          represented by m m m k kin which m and k are each a propylene unit,              
                                          1                                           