Appeal No. 1998-0215 Application No. 08/052,671 glycol thermoplastic resin, said resin being bonded to the fiberglass strands and being present in amounts operable to bond overlapping knuckles of the woven fiberglass together, and to prevent significant fraying of cut edges of said sheet or tape, and to form a remeltable and resolidifiable bondable thermoplastic surface on the cloth. PRIOR ART In support of her rejections, the examiner relies on the following prior art references : 1 Pedlow 4,018,962 Apr. 19, 1977 Wade, Jr. et al. (Wade) 4,761,520 Aug. 2, 1988 Mater et al. (Mater) 5,118,558 Jun. 2, 1992 Yoshimi et al. (Yoshimi ) 63-7602 2 Jan. 13, 1988 (published Japanese Kokai Patent Application) REJECTION The appealed claims stand rejected as follows:3 1Our reference to the published Kokai Japanese application is to the corresponding English translation of record. 2The examiner refers to it as “Nihon Radiator” at page 2 of the Answer. 3The examiner has withdrawn § 112 rejections set forth in the final Office action dated March 3, 1994 (Paper No. 6) and the first Supplemental Examiner’s Answer dated August 8, 1996 (Paper No. 16), respectively. See page 2 of the Answer dated September 18, 1995 (Paper No. 13) and page 1 of the second Supplemental Examiner’s Answer dated July 8, 1997 (Paper No. 4Page: Previous 1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 NextLast modified: November 3, 2007