                            wherein M equals  Sn, Ti, Fe, Cu, Nb, Ta, Co, Ni, Mg,                                        
                                          Li, Na, Ga and mixtures thereof,                                               
                                   a    is from about 0.5 to about 5.0,                                                  
                                   b    is from about 0.1 to 5.0, and                                                    
                                   x    is the number of oxygen atoms required to                                        
                                   satisfy the valency requirement of the other                                          
                                   elements.                                                                             
                     comprising (1) mixing the vanadium compound, at least a portion of the                              
                     antimony compound, and at least a portion of the M compound and an                                  
                     aqueous sol containing a portion of the support material to form an aqueous                         
                     slurry, heating the slurry to remove the water, and calcining at a temperature                      
                     of at least about 150°C to form a catalyst precursor; (2) mixing the catalyst                       
                     precursor with an aqueous sol containing the remaining portion of the                               
                     support for the catalyst and any remaining portion of the Sb compound and M                         
                     compound to form a second slurry; (3) drying the second slurry to remove                            
                     the water to form a dry mixture; and (4) calcining the dried mixture at a                           
                     temperature of at least 150°C to form the finished catalyst.                                        
                     As evidence of unpatentability of the claimed subject matter, the Examiner relies on                
              the following references:                                                                                  
              Brazdil et al. (Brazdil ‘016)      5,214,016             May 25, 1993                                      
              Brazdil et al. (Brazdil ‘588)      5,498,588             Mar. 12, 1996                                     








                                                           -3-                                                           





Page:  Previous  1  2  3  4  5  6  7  8  Next 

Last modified: November 3, 2007