            1.  A process for producing "-alumina by calcining a                                       
            transition alumina obtained by calcination of aluminum hydroxide                           
            prepared by hydrolysis of alumina isopropoxide in an atmosphere                            
            containing at least 10% of volume of hydrogen chloride, at a                               
            temperature of from 700 to 1,300oC, at atmosphere pressure and                             
            for a calcining time of from 10-120 minutes to produce said "-                             
            alumina.                                                                                   