Appeal No. 1999-2507 Application No. 08/967,367 in which n is a number from 2 to 10, and 0 to 99% by weight, based on the total weight of cycloolefin polymer, of one or more acyclic olefins of the formula VIII in which R9, R10, R11 and R12 are identical or different and are a hydrogen atom or a C1-C20 hydrocarbon radical; and said particulate core/shell component consisting essentially of: one or more rubber phase(s) and one or more hard phase(s), the hard phase having a glass transition temperature above 50°C and the rubber phase having a lower glass transition temperature than said hard phase, said rubber and hard phases consisting essentiall y of polymerize dunsaturate dcompounds having carbon- carbon bonds in the polymer backbone. 14. A polymer alloy comprising: (a) a cycloolefin copolymer component comprising a copolymer of the reactants comprising norbornene or tetracyclododecene and an acyclic olefin, and dispersed in said cycloolefin copolymer component, (b) a particulate core/shell component comprising at least one rubbery phase having a glass transition temperature below 0°C and a hard phase having a glass transition temperature above 50°C; the rubbery phase consisting essentially of, or, if more than one rubbery phase is present in said alloy, each said rubbery phase consisting essentially of one or more polymerized unsaturated 14Page: Previous 1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 NextLast modified: November 3, 2007