Appeal No. 2002-0258 Application No. 09/254,402 at least one electrochemical solid electrolytic test cell including at least one cathode; a selective oxygen-ion-conductive layer covering the at least one cathode and including a mixed-conductive ceramic material, the selective oxygen-ion-conductive layer being exposed to the gas mixture and being configured to conduct oxygen therethrough only in the form of oxygen ions; and an electrically nonconductive layer separating the at least one cathode from the selective oxygen-ion-conductive layer, the electrically nonconductive layer including particular portions which are permeable to gas, the gas-permeable portions being configured to conduct the oxygen conducted through the selective oxygen-ion-conductive layer to the cathode; wherein the cathode is separated from the gas mixture by the selective oxygen-ion-conductive layer and the electrically nonconductive layer. 12. The measuring arrangement according to claim 11, further comprising: at least one further cathode, wherein the at least one cathode is situated in a diffusion channel between an opening of the diffusion channel and the at least one further cathode. 18. The measuring arrangement according to claim 12, wherein the diffusion channel is a tunnel structure composed of heat- resistant glass. The References In rejecting the claims under 35 U.S.C. § 103(a), the examiner relies upon the following references: Nakazawa et al. (Nakazawa) 5,178,744 Jan. 12, 1993 Garzon et al. (Garzon) 5,543,025 Aug. 06, 1996 Liu et al. (Liu) 5,667,652 Sep. 16, 1997 Dietz et al. (Dietz) 5,879,526 Mar. 09, 1999 2Page: Previous 1 2 3 4 5 6 7 8 9 NextLast modified: November 3, 2007