Appeal 2006-2330 Application 10/364,089 35. A method of forming a coated laminate including a first ply and a second ply, both having a major surface, comprising the steps of: depositing a first anti-reflective layer over at least a portion of the major surface of either the first or second ply; depositing a first infrared reflective film over the first anti-reflective layer having a thickness ranging from 25 Å to 300 Å; depositing a second anti-reflective layer over the first infrared reflective film; depositing a second infrared reflective film over the second anti-reflective layer having a thickness ranging from 25 Å to 150 Å; depositing a third anti-reflective layer over the second infrared reflective film; and depositing a third infrared reflective film over the third anti-reflective layer having a thickness ranging from 50 Å to 100 Å, wherein the second infrared reflective film is thicker than the third infrared reflective film. 41. A coated, laminated article, comprising: a first ply having a major surface; a second ply having a major surface; and a coating deposited on at least a portion of the major surface of either the first or second ply comprising a first anti-reflective layer, a first infrared reflective film deposited over the first anti-reflective layer having a thickness ranging from 25 Å to 300 Å, 3Page: Previous 1 2 3 4 5 6 7 8 9 10 11 12 NextLast modified: November 3, 2007