Appeal 2006-2330 Application 10/364,089 a second anti-reflective layer deposited over the first infrared reflective film, a second infrared reflective film deposited over the second anti-reflective layer having a thickness ranging from 25 Å to 150 Å, a third anti-reflective layer deposited over the second infrared reflective film, and a third infrared reflective film deposited over the third anti-reflective layer having a thickness ranging from 50 Å to 100Å, wherein the second infrared reflective film is thicker than the third infrared reflective film, the infrared reflective films have a sheet resistance in the range of 1.5 to 3 ohms per square. 53. A method of improving the solar control properties of a laminated article including a first ply and a second ply containing a coating having three or more infrared reflective films on either the first or second ply, comprising: heating the coating to a temperature sufficient to obtain a sheet resistance in the range of 1.5 to 3 ohms per square for the infrared reflective films. References Relied on by the Examiner The Examiner relies upon the following references as evidence of unpatentability: Weber US 4,940,495 Jul. 10, 1990 Depauw US 6,090,481 Jul. 18, 2000 Okamura US 6,104,530 Aug. 15, 2000 Noethe US 6,572,940 B1 Jun. 3, 2003 Lingle US 6,576,349 B2 Jun. 10, 2003 4Page: Previous 1 2 3 4 5 6 7 8 9 10 11 12 NextLast modified: November 3, 2007