           1          14. Watanabe discloses a non-aqueous electrolyte secondary battery                      
           2                 comprising a lithium-containing silicon oxide electrode as a                     
           3                 negative electrode, either a lithium-containing titanium oxide or                
           4                 lithium-containing iron sulfide as a positive electrode, and a                   
           5                 non-aqueous electrolyte.  (Watanabe, 3:45-50.)                                   
           6          15. Watanabe teaches that the negative electrode may contain non-                       
           7                 metals such as carbon in addition to the lithium-containing                      
           8                 silicon oxide and specifically discusses the use of calcined                     
           9                 carbonaceous compounds capable of absorbing and releasing                        
          10                 lithium ion or lithium metal.  (Watanabe, 6:2-14, 7:37-40.)                      
          11          16. Watanabe also teaches that the positive electrode material may                      
          12                 contain other metals such as nickel and manganese in addition                    
          13                 to lithium and titanium.  (Watanabe, 8:22-34.)                                   
          14          17. Watanabe discloses the use of lithium salts such as lithium                         
          15                 phosphorus hexafluoride (LiPF6) as the electrolyte.  (Watanabe,                  
          16                 12:44-46.)                                                                       
          17          18. Watanabe discloses the desirability of the battery to be                            
          18                 assembled in a moisture-free atmosphere. (Watanabe, 14:37-                       
          19                 38.)                                                                             
          20          19. Watanabe discloses the moisture content to be preferably 2,000                      
          21                 ppm or less for the entire battery and 50 ppm for the positive                   
          22                 electrode mixture, the negative electrode mixture, or the                        
          23                 electrolyte from the point of cycle property.  (Watanabe, 14:47-                 
          24                 51.)                                                                             