                             Mr. Hess testified that in 1987 he was the operation lead of the product                        
              development lab and oversaw the testing (molding test samples, Izod Impact testing,                            
              making test chips, and conducting Kasha Index measurements), and that he wrote weekly                          
              reports on the amount of work that went through the lab.  HR 287 and 288.  He testified that                   
              he supervised the compounding of resin powders into pellets.  HR 290.  He testified that                       
              HX 3 is a request, dated July 13, 1987, from Dr. Cooper to extrude a sample of the para-                       
              cumyl phenol endcapped polycarbonate resin powder (RL 5568)  into pellets, some being                          
              compounded with a stabilizer R 542 and some compounded with a mold release agent R                             
              538 and to extrude a parallel sample of RL 5404 (a similar grade of polycarbonate resin                        
              endcapped with para-tertiary butyl phenol).  Mr. Hess testified that in accordance with the                    
              request, Mr. Butler, a technician, now deceased, working under Mr. Hess’ direction and                         
              supervision, extruded six batches, three for each resin.  HR 291 to 303; HX 3 and 10.  Mr.                     
              Hess testified that each of the six batches was tested on July 23 and 24, 1987, for its                        
              Kasha Index measurement; that the Kasha Index test is a simple, routine and regularly                          
              conducted test; that the results show that each batch had a Kasha Index value falling in the                   
              range between 2800 and 3400 at 250EC; that the results were recorded in log book (HX                           
              11); and that  he is the custodian of the record.  HR 303 to 308.  He also testified that the                  
              six extrusion batches (para-cumyl phenol versus para-tertiery butyl phenol endcapped disc                      
              resins) identified in HX 3 were prepared for ductile/brittle transition testing (notched Izod                  