Ex parte RIES et al. - Page 3




          Appeal No. 1996-3659                                                        
          Application No. 08/237,484                                                  

               1. A vapor deposition method for coating a substrate with              
          a porous zeolitic film, the method comprising the steps of:                 
                    (a) irradiating a porous zeolite with a pulsed laser              
               beam of at least sufficient duration and intensity to                  
                    vaporize the zeolite in a three-dimensional plume                 
          adjacent       to the zeolite; and                                          
                    (b) intercepting the plume on the substrate to form               
          the       porous zeolitic film.                                             
               10. A sensor, comprising:                                              
                    (a) a piezoelectric substrate; and                                
                    (b) a porous zeolitic film coated on the                          
          piezoelectric       substrate, the porous zeolitic film formed              
          by irradiating a    porous zeolite with a pulsed laser beam of              
          at least            sufficient duration and intensity to                    
          vaporize the zeolite in       a three-dimensional plume                     
          adjacent to the zeolite and then        intercepting the plume              
          on the substrate to form the porous     zeolitic film.                      
                              THE REFERENCES OF RECORD                                
          As evidence of obviousness, the examiner relies upon the                    
          following references:                                                       
          Venkatesan et al.        5,015,492                May  14, 1991             
          (Venkatesan)                                                                
          Bein et al.              5,151,110                Sep. 29, 1992             
          (Bein)                                                                      
          Bals et al.              5,331,845                Jul. 26, 1994             
          (Bals)                        (filed Jan. 19, 1993)                         
          Böszörményi et al. (Boszormenyi), “Model silica-alumina acid                
          catalysts for surface science and catalysis studies prepared                

          inclusion in the Appendix is considered inadvertent.                        