               The subject matter on appeal relates to a method of                   
          producing a motor vehicle body panel from aluminum alloy sheet.            
          Further details of this appealed subject matter are recited in             
          illustrative claims 1 and 14 reproduced below:                             
                    1.  A method of producing a motor vehicle body                   
               panel from aluminum alloy sheet comprising,                           
                    roll casting an aluminum alloy strip having a                    
               thickness of less than about 0.5 inch,                                
                    cold rolling said strip to a thickness of less                   
               than about 0.15 inch,                                                 
                    effecting said cold rolling of said cast strip                   
               without prior thermal treatment of said roll cast                     
               strip,                                                                
                    subjecting said cold rolled strip to continuous                  
               annealing at a temperature of about 750ºF to 1000ºF                   
               for about 1 to 60 seconds,                                            
                    subsequent to said continuous annealing                          
               converting said strip into a motor vehicle body panel,                
               and                                                                   
                    said aluminum alloy being an alloy selected from                 
               the group consisting of 3XXX and 5XXX.                                
                    14.  A method of producing a motor vehicle body                  
               panel from aluminum alloy sheet comprising,                           
                    roll casting an aluminum alloy strip having a                    
               thickness of less than about 0.5 inch,                                
                    cold rolling said strip to a thickness of less                   
               than about 0.15 inch,                                                 
                    effecting said cold rolling of said roll strip                   
               without prior thermal treatment of said cast strip,                   
                    subjecting said cold rolled strip to solution                    
               heat treatment at a temperature of about 800ºF to                     
               1100ºF for about 1 to 60 seconds,                                     



                                                                                     
          and 14.  According to the advisory action of March 26, 1998                