Appeal No. 2006-0415 Application No. 10/267,200 1 REPRESENTATIVE CLAIM 2 The sole independent claim is as follows: 3 27. A method of preparing a flexible film laminate 4 comprising: 5 a) mixing an epoxy resin and a curative having at least one 6 active hydrogen contained in a functional group selected from the 7 group consisting of primary amino groups, secondary amino groups, 8 carboxyl groups and combinations thereof to form an adhesive 9 formulation, said epoxy resin and said curative having been 10 selected so as to maintain the viscosity of said adhesive 11 formulation for at least 20 minutes after mixing within the range 12 of 1,000 to 10,000 cps at 40°C and said adhesive formulation being 13 essentially free of solvent, water and isocyanate-functionalized 14 compounds; 15 b) applying the adhesive formulation to a surface of a first 16 substrate selected from the group consisting of metal foils and 17 polymeric films; 18 c) pressing said surface of said first substrate having the 19 adhesive formulation applied thereto against a surface of a second 20 substrate selected from the group consisting of metal foils and 21 polymeric films; and 22 d) curing the adhesive formulation. 23 2Page: Previous 1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 NextLast modified: November 3, 2007